TMT bars are specified under IS 1786. The grade number is the minimum yield stress in N/mm2; the D suffix means tighter ductility requirements, which matter in earthquake zones.

Cost tiers are RELATIVE only (lower / medium / higher). SPSDPS does not publish current prices - get written local quotations.

The short answer

Use the grade and size your structural engineer specifies. Ductility (the "D" grades) matters in earthquake zones.

If your situation is this, choose that
If you need...ConsiderWhy
Earthquake-prone area or engineer specifies ductile barsFe 500D or Fe 550DThe D marks higher ductility so a structure bends before it breaks.
Ordinary non-structural or minor workFe 500 / Fe 415Follow the drawing; never swap grade without the engineer.
Not sureUse the grade printed on the structural drawingSubstituting steel changes the design.

All options at a glance

All options at a glance
OptionRelative costBest forWatch out for
Fe 415 / 415DLowerWhere the design specifically calls for it.Lower strength per bar than Fe 500
Fe 500MediumGeneral RCC where the design specifies Fe 500.Standard ductility only
Fe 500DMedium to higherEarthquake-prone regions and where D grade is specified.Costs more than Fe 500
Fe 550DHigherDesigns that specify Fe 550D.Only valid if the design uses 550

Compare side by side

Choose up to 3 to compare

The check mark shows an option that has figures verified against a cited source.

Fe 415 / 415D

Standard: IS 1786

Relative cost: Lower

Specifications

  • Minimum yield / 0.2% proof stress

    415 N/mm2

    Verified- InfraLens

Advantages

  • Easier to bend
  • Common in older designs

Disadvantages

  • Lower strength per bar than Fe 500

Best for

Where the design specifically calls for it.

Avoid

Substituting for a higher grade without engineer approval.

Fe 500

Standard: IS 1786

Relative cost: Medium

Specifications

  • Minimum yield / 0.2% proof stress

    500 N/mm2

    Verified- InfraLens

Advantages

  • Widely used grade
  • Good strength-to-weight

Disadvantages

  • Standard ductility only

Best for

General RCC where the design specifies Fe 500.

Avoid

Where ductile (D) grade is specified.

Fe 500D

Standard: IS 1786

Relative cost: Medium to higher

Specifications

  • Minimum yield / 0.2% proof stress

    500 N/mm2

    Verified- InfraLens

  • Difference from Fe 500

    Tighter ductility requirements (higher elongation and UTS/YS ratio)

    Verified- InfraLens

Advantages

  • Better ductility for seismic performance
  • Same yield as Fe 500

Disadvantages

  • Costs more than Fe 500

Best for

Earthquake-prone regions and where D grade is specified.

Avoid

Assuming it replaces proper ductile detailing.

Common mistakes

  • Choosing a cheaper unbranded bar without a test certificate.
  • Using rusted, oily or bent-and-rebent bars.
  • Cutting cover or lap lengths on site to save steel.

Ask the shop

  • Is the manufacturer's test certificate provided with the lot?
  • Is the grade rolled into each bar?
  • Can I see the weight per metre for the diameter?

Words you will hear

Fe 500
Steel with 500 MPa minimum yield strength.
Ductility
Ability to stretch without snapping.
Lap length
Overlap needed where two bars join.

Next steps

How to choose

  • The structural drawing decides the grade - never substitute without the engineer.
  • Ask for the mill test certificate and check the BIS mark and heat number.
  • Check bars for rust scale, bends and cracks before use.
  • Store bars off the ground and covered.

Sources and how far to trust them

Limits of this comparison: Only minimum yield values were verified. Tensile strength, elongation and UTS/YS ratios must be read from the current IS 1786 edition. IS 13920 governs ductile detailing in seismic design.

Standards are revised. Confirm any value you rely on against the current edition on the BIS website. Information is for planning, not a specification.